很多门窗厂把返修怪到合片工身上,其实双道密封里真正扛气密的是第一道丁基胶。胶条断线、宽窄不一、铝条转角堆胶,装进窗框半年就开始起雾——问题全出在涂布那几秒。
Many door and window factories blame the repair on the laminating workers, but in fact, the first layer of butyl rubber is the one that truly holds the airtightness in the double seal. The glue strip is broken, the width is uneven, and the aluminum strip corner is stacked with glue. It starts fogging after half a year of installation in the window frame - the problem lies entirely in the few seconds of coating.

立式机型把铝间隔框竖着送进去,双压轮定位、光电触发出胶,单人就能连续干,非常适合家装门窗和中型工程单。
The vertical model vertically feeds the aluminum spacer frame in, with dual pressure wheel positioning and photoelectric triggered glue dispensing. It can be continuously dried by a single person, especially suitable for home decoration doors and windows and medium-sized engineering projects.
挑设备别只看“能不能出胶”,盯死这四点:
Don't just look at whether the equipment can produce glue, focus on these four points:
胶缸和胶头分开控温:冬天胶稠、夏天胶稀,只有双区独立恒温,出胶宽度才稳在3.5–4.5mm,不堆胶也不露底。
Separate temperature control for the glue tank and glue head: glue is thick in winter and thin in summer. Only with dual zone independent constant temperature can the glue width be stable at 3.5-4.5mm, without stacking glue or exposing the bottom.
胶头间距免泄压调节:换4mm、6mm、暖边条不用停机放压,手轮一转就行,小批量多规格订单非常省时间。
Rubber head spacing adjustment without pressure relief: Changing to 4mm, 6mm, or warm edge strips does not require stopping the machine to release pressure, just one turn of the handwheel is enough, saving time for small batch and multi specification orders.
液压增压别用纯气动:10–17MPa挤胶压力要稳,气动便宜但压力抖,胶条容易一段粗一段细。
Do not use pure pneumatic for hydraulic boosting: the extrusion pressure should be stable at 10-17MPa. Pneumatic is cheap but the pressure is unstable, and the rubber strip is prone to thicker and thinner sections.
带定时加热和一键洗胶:上班前自动预热,下班不用等降温;堵胶时自动回流清洗,别让师傅拿铁丝捅胶嘴。
Equipped with timed heating and one click glue washing: automatic preheating before work, no need to wait for cooling after work; When blocking the glue, it will automatically flow back for cleaning. Do not let the master poke the glue nozzle with wire.
顺手避两个坑:传送带选耐高温片基带,别用普通PU带,长期烤会拉长跑偏;买之前拿自己常用的铝条和丁基胶去厂家现场试一分钟,看四个转角有没有断点和气泡,比看彩页实在。
Avoid two pitfalls: choose a high-temperature resistant sheet base belt for the conveyor belt, do not use ordinary PU belts, as long-term baking will cause elongation and deviation; Before making a purchase, take your commonly used aluminum strip and butyl rubber to the manufacturer's site for a one minute trial to see if there are any breaks or bubbles at the four corners, which is more practical than looking at the brochure.
济南本地有整机装配和胶路配件的厂子,后期换胶嘴、密封圈不用等快递,停机半天就能恢复。
There are local factories in Jinan that assemble complete machines and rubber road accessories. In the later stage, there is no need to wait for express delivery to replace the rubber nozzle and seal ring. It can be restored after half a day of shutdown.
本文由立式丁基胶涂布机友情奉献.更多有关的知识请点击:http://www.jncsjx.com我们将会对您提出的疑问进行详细的解答,欢迎你登录网站留言.
This article is a friendly contribution from a vertical butyl rubber coating machine For more information, please click: http://www.jncsjx.com We will provide detailed answers to your questions. You are welcome to log in to our website and leave a message
- 折弯先看回弹量 2026/11/16
- 封胶线先看转角 2026/11/14
- 灌分子筛的隐形时钟 2026/11/12
- 一条线跑顺,先别只盯“全自动”三个字 2026/11/09
- 涂得准却压不上,卡在工序接缝那几秒 2026/11/06
- 胶条断在第三边,锅不一定在机器 2026/11/04
- 0.5毫米的偏差,整窗质保直接归零 2026/11/02
- 别看参数表,先看今天车间里堆的是哪种框 2026/10/30
- 中空玻璃漏不漏气,第一道胶就定了生死 2026/10/28
- 中空玻璃起雾,八成是第一道胶没涂稳 2026/10/26

当前位置:



产品分类Product categories
联系我们Contact us